Fits: Clearance, Transition and Interference — the Difference Is Microns
Martin

Создано

Martin

24. сентябрь 2026NO
25
0
0
0
0

Fits: Clearance, Transition and Interference — the Difference Is Microns

A shaft that slides into a hole and a shaft that has to be pressed in can differ in diameter by less than the thickness of a human hair. Which of those you have is decided by a few microns, and the difference in behaviour is total. A CLEARANCE fit always has a gap: the parts assemble by hand and can move. An INTERFERENCE fit always has the shaft larger than the hole: the parts must be forced together and then grip each other permanently. A TRANSITION fit may be either, depending on where the two parts happen to fall in their tolerances. This is why a bearing can spin on its shaft, or crack its outer ring, or work perfectly — all from the same drawing and the same parts bin. The fit is the design decision, and it is made in numbers before anything is cut.
Средний
3 hours

Инструкции

1

Measure both parts, and measure them properly

You cannot choose a fit without knowing what you have. Measure the shaft and the bore with a micrometer or a good caliper, at several places along their length and at several angles round them. Several angles matters because nothing is perfectly round. A shaft that reads 19.98 mm one way and 20.02 mm at ninety degrees is out of round by 0.04 mm, which is larger than most fits — and averaging the two hides it. Let both parts reach the same temperature first. Steel expands about 11 microns per metre per degree, so a 50 mm part handled for a minute can grow by more than the fit you are trying to measure. Warm hands are a real error here.

Материалы для этого шага:

Стальной вал 30 ммСтальной вал 30 мм1 штука

Необходимые инструменты:

ШтангенциркульШтангенциркуль
Цифровой штангенциркуль 6 дюймовЦифровой штангенциркуль 6 дюймов
2

The arithmetic, and what each fit is for

Загрузка блокнота Jupyter…

Материалы для этого шага:

Стальной вал 30 ммСтальной вал 30 мм1 штука
Ball Bearing - Non-Flanged (8mm Bore, 22mm OD)Ball Bearing - Non-Flanged (8mm Bore, 22mm OD)1 штука

Необходимые инструменты:

ШтангенциркульШтангенциркуль
Настольный компьютерНастольный компьютер
КалькуляторКалькулятор
3

Temperature is a tool, not just an error

Heat the outer part and it grows; chill the inner part and it shrinks. Do both and an interference fit can be assembled by hand, then locks as the temperatures equalise. Steel expands about 11 microns per metre per degree Celsius, so a 100 mm bore heated by 100 degrees grows roughly 0.11 mm — far more than any normal interference. An oven at 120 degrees, or a freezer for the shaft, is usually enough. Never heat a bearing above about 120 degrees. Above that the hardened rings begin to temper and lose hardness permanently, and a blowtorch anywhere near a bearing ruins it in seconds. Induction heaters and hot oil baths exist precisely because the temperature has to be controlled.

Материалы для этого шага:

Стальной вал 30 ммСтальной вал 30 мм1 штука
Ball Bearing - Non-Flanged (8mm Bore, 22mm OD)Ball Bearing - Non-Flanged (8mm Bore, 22mm OD)1 штука

Необходимые инструменты:

Цифровой штангенциркуль 6 дюймовЦифровой штангенциркуль 6 дюймов
Нитриловые перчаткиНитриловые перчатки
4

Surface finish and roundness are part of the fit

A measured diameter is an average over a surface that has peaks and valleys. Press two rough surfaces together and the peaks flatten, so the effective interference is less than the measured one — often by 2 to 5 microns on ordinary turned work. That is why bearing seats are ground rather than turned. It is not fussiness: a rough seat loses a significant fraction of a 15 micron interference to flattened peaks the first time the joint is loaded, and then the bearing creeps. Roundness matters as much. A bore that is 0.03 mm oval will grip a round shaft at two points and leave gaps at ninety degrees, so the pressure is concentrated rather than shared — which distorts the bearing ring and takes the internal clearance with it.

Материалы для этого шага:

Стальной вал 30 ммСтальной вал 30 мм1 штука

Необходимые инструменты:

Индикатор часового типаИндикатор часового типа
ШтангенциркульШтангенциркуль
Набор щуповНабор щупов

Материалы

2

Требуемые инструменты

7
Предполагаемая сумма
То, что купил мастер. Материалы без цены вы покупаете там, где найдёте.
$1.27

CC0 Общественное достояние

Этот чертёж выпущен под лицензией CC0. Вы можете свободно копировать, изменять, распространять и использовать эту работу в любых целях без запроса разрешения.

Поддержите мейкера, покупая товары через его чертёж, где он получает Комиссию мейкера установленную продавцами, или создайте новую итерацию этого чертежа и включите его как связь в свой чертёж для распределения дохода.

Обсуждение

(0)

Войти чтобы присоединиться к обсуждению

Загрузка комментариев...