Oxidising, Neutral and Reducing: What the Fire Does to the Work
Forge

Создано

Forge

24. сентябрь 2026NO
1
0
0
0
0

Oxidising, Neutral and Reducing: What the Fire Does to the Work

A fire is a chemical environment, not just a source of heat, and it changes the work while it heats it. Too much air and the surface oxidises and burns away; too little and the fire is cool and sooty; in between it does almost nothing to the steel. Smiths call these OXIDISING, REDUCING and NEUTRAL. Potters call them the same and use them deliberately — a reduction firing is how copper glazes turn red and celadon turns green, which is a chemical effect rather than a colour choice. Recognising which one you have is a matter of looking at the flame and the work, and it is directly controllable with the air.
Средний
3 hours

Инструкции

1

Recognising the three by eye

An OXIDISING fire has excess air: the flame is short, clear and blue-tinged, the fire looks clean, and the work scales heavily and sparkles at high heat. A REDUCING fire has excess fuel: the flame is long, lazy and yellow with a smoky tip, there is visible flame licking out of the top of the fuel bed, and the work comes out relatively clean and dark. NEUTRAL sits between and is what most forging wants. Move the blast up and down and watch the flame change — half a minute doing that teaches the three states better than any description, and after that you will recognise them without thinking.

Материалы для этого шага:

Древесный уголь кусковойДревесный уголь кусковой2 штук
Пруток из низкоуглеродистой сталиПруток из низкоуглеродистой стали1 штука

Необходимые инструменты:

Кузнечный горнКузнечный горн
Меха (кузнечные)Меха (кузнечные)
Затемнённые очки для горнаЗатемнённые очки для горна
2

Scale: what an oxidising fire costs you

Every heat in an oxidising fire converts some of the surface to iron oxide — SCALE — which flakes off on the anvil. That metal is gone permanently, and on a piece reheated many times the loss is significant. It also damages the surface. Scale hammered into hot steel leaves pits that have to be ground or filed out later, which costs more metal again. Brushing the work before each blow keeps the surface clean and is the reason a wire brush lives beside every anvil. A reducing fire produces far less scale, which is one reason forge welding is done in one: the surfaces must be clean and oxide-free at the moment they are joined, and an oxidising fire is actively working against that.

Материалы для этого шага:

Пруток из низкоуглеродистой сталиПруток из низкоуглеродистой стали1 штука

Необходимые инструменты:

Кузнечный горнКузнечный горн
НаковальняНаковальня
Кузнечный молотКузнечный молот
Кузнечные клещиКузнечные клещи
3

Decarburisation: the damage you cannot see

At high temperature in an oxidising atmosphere, carbon is drawn out of the surface layer of steel. The metal is still there; its carbon is not. That layer will not harden. A blade held too long at high heat in a dirty fire can be decarburised a few tenths of a millimetre deep, quench perfectly, and still have a soft edge — and nothing about its appearance reveals this before the hardness test fails. Keep high-carbon steel out of oxidising conditions, minimise the time at temperature, and leave enough stock to grind the surface layer away afterwards. This is the failure most often misdiagnosed as a bad quench.

Материалы для этого шага:

Пруток из низкоуглеродистой сталиПруток из низкоуглеродистой стали1 штука

Необходимые инструменты:

Кузнечный горнКузнечный горн
Термопара с индикаторомТермопара с индикатором
Ювелирная лупаЮвелирная лупа
4

Deliberate reduction: when the atmosphere is the point

Potters reduce on purpose. Starving the kiln of oxygen pulls it out of the metal oxides in the glaze instead, and copper that would be green in oxidation turns blood red, while iron gives celadon green rather than tan. It is the same chemistry that smelting depends on: a reducing atmosphere is what takes the oxygen out of iron ore and leaves metallic iron. The published bloomery and smelting blueprints are this effect used at its largest scale. The control is the same everywhere — restrict air, add fuel. What differs is only what you are trying to reduce, and whether you want the effect on the surface of a pot, throughout a glaze, or in a furnace full of ore.

Материалы для этого шага:

Древесный уголь кусковойДревесный уголь кусковой2 штук

Необходимые инструменты:

Муфельная печьМуфельная печь
Высокотемпературная печьВысокотемпературная печь
Угольная печьУгольная печь
БлокнотБлокнот

Материалы

2

Требуемые инструменты

12

CC0 Общественное достояние

Этот чертёж выпущен под лицензией CC0. Вы можете свободно копировать, изменять, распространять и использовать эту работу в любых целях без запроса разрешения.

Поддержите мейкера, покупая товары через его чертёж, где он получает Комиссию мейкера установленную продавцами, или создайте новую итерацию этого чертежа и включите его как связь в свой чертёж для распределения дохода.

Обсуждение

(0)

Войти чтобы присоединиться к обсуждению

Загрузка комментариев...