Varnish and Polyurethane: Thin Coats, and Leave It Alone
Polyurethane is the toughest finish most workshops will use: genuinely water resistant, genuinely abrasion resistant, and the right answer for a worktop, a floor or a table that gets used.
It is also the least forgiving to apply. It stays wet long enough to collect dust, it shows every brush mark, and each coat is a separate layer rather than melting into the last — so a sand-through is visible as a witness line forever.
Two rules cover nearly all of it: thin coats, and stop touching it. Almost every bad polyurethane finish comes from a thick coat or from brushing back over one that had started to set.
متوسط
4 hours
التعليمات
1
1
Oil-based or water-based: pick for colour and smell, not for toughness
Oil-based or water-based: pick for colour and smell, not for toughness
OIL-BASED cures slowly, flows out well so brush marks level themselves, warms the colour of the wood, and continues to yellow for years. It smells strongly and needs solvent to clean up.
WATER-BASED dries in a couple of hours, stays water-clear so pale timbers stay pale, has little odour and cleans up with water. It levels less well, so brush marks are more likely, and it raises the grain on the first coat — which the surface rung pre-empts by raising the grain deliberately.
Modern water-based products are comparable in durability, so the honest basis for choosing is colour, dry time and smell. Do not use them over an oil finish that has not fully cured, and seal an oily or resinous timber with dewaxed shellac first.
المواد لهذه الخطوة:
بولي يوريثان - أساسه الزيت1 قطعة
بولي يوريثان - أساسه الماء1 قطعة
لوح خشب صلب2 قطعالأدوات المطلوبة:
فرشاة دهان عريضة
فرشاة إسفنجية
قفازات نتريل2
2
Thin it, and wipe rather than brush
Thin it, and wipe rather than brush
A WIPING varnish — polyurethane thinned by half with mineral spirits and wiped on with a cloth — is the most reliable way for a beginner to get a good film finish, and it is what many 'wipe-on poly' products already are.
Thin coats cannot run, cannot sag, hold far less dust because they set quickly, and show no brush marks because there is no brush. The cost is that you need more of them — five or six rather than two or three — and each is quick.
If you brush, use a good brush, load it properly, lay the finish on in one direction and tip off lightly along the grain. Then stop. A brush going back into partly set varnish tears it, and that tear is permanent.
المواد لهذه الخطوة:
بولي يوريثان - أساسه الزيت1 قطعة
سبيرتو معدني1 قطعةالأدوات المطلوبة:
قماش قطني
فرشاة دهان عريضة
قفازات نتريل3
3
Between coats: scuff, do not sand through
Between coats: scuff, do not sand through
Once a coat is properly dry, knock off dust nibs with very fine abrasive or a grey pad, wipe clean, and apply the next. The scratches give the next coat something to key to, which polyurethane needs because it does not dissolve into the previous layer.
Use light pressure and stay off the edges. Edges have the thinnest film and sand through first, and a sand-through on a stained surface takes the colour with it — leaving a pale patch that cannot be blended.
Respect the recoat window on the tin. Recoat too early and the solvent in the new coat softens and wrinkles the one beneath; leave it far too long and the new coat will not bond well, which is what the scuffing is compensating for.
المواد لهذه الخطوة:
تشكيلة وسائد Scotch-Brite1 قطعة
تشكيلة ورق صنفرة1 قطعةالأدوات المطلوبة:
قماش التقاط الغبار
طقم قوالب صنفرة (إسفنج)
عدسة صائغ4
4
Dust, temperature and the last coat
Dust, temperature and the last coat
Oil-based polyurethane stays wet for hours, and everything floating in the air lands on it. Vacuum beforehand, let the air settle, do not sweep, and if you can, finish in a different room from the one you sanded in.
Temperature matters more than people expect. Too cold and it will not cure properly; too warm and it skins before it levels, leaving brush marks set in place. Check the range on the tin and believe it.
Leave the last coat alone completely. Full cure takes days even though it feels dry in hours, and a surface put into use too early prints, dents and marks in ways it never would once hard. For a high build, rub the cured film out with fine abrasive and wax — which the next rung covers — rather than trying to lay a perfect final coat.
المواد لهذه الخطوة:
بولي يوريثان - أساسه الزيت1 قطعةالأدوات المطلوبة:
قماش التقاط الغبار
فرشاة دهان عريضةالمواد
6- عنصر نائب
- عنصر نائب
- 2 قطععنصر نائب
- 1 قطعةعنصر نائب
- تشكيلة وسائد Scotch-Briteعمولة 10%1 قطعةعنصر نائب
- 1 قطعةعنصر نائب
المخططات ذات الصلة
هذه المخططات تشارك المعرفة مع هذا — التقنيات والمواد والمبادئ
CC0 ملكية عامة
هذا المخطط مُصدر بموجب CC0. يحق لك نسخه وتعديله وتوزيعه واستخدامه لأي غرض، دون طلب إذن.
ادعم الصانع بشراء منتجات عبر مخططه حيث يكسب عمولة الصانع يحددها البائعون، أو أنشئ نسخة جديدة من هذا المخطط وضمّنه كرابط في مخططك لمشاركة الإيرادات.