Cemented Carbide
Tungsten carbide is nearly as hard as diamond and, on its own, useless: a pressed block of it shatters. The invention is not the carbide. It is the idea of cementing hard carbide grains in a small amount of tough metal, so the composite keeps most of the hardness and borrows the metal's resistance to cracking.
German patent DRP 420,689, filed 1923 by Osram Studiengesellschaft, for a method by Karl Schröter: hard materials made by pressing and sintering tungsten monocarbide with 10-20 weight-per-cent of an iron-group metal — iron, nickel or cobalt — with the binder briefly liquid so the mass densifies into a solid body. Krupp bought the patent in 1926 and marketed the product worldwide from 1927 as WIDIA, from wie Diamant, “like diamond”.
Osram's interest was not machining at all. They needed hard dies for drawing tungsten lamp filaments, and diamond dies were scarce and expensive. The cutting-tool industry was a side-effect.
Інструкції
Write the composite idea down
Write the composite idea down
One line: hard grains carry the cutting, a tough binder carries the load. Neither component alone would work.
Необхідні інструменти ({count})
Notebook and PencilWeigh the carbide blank
Weigh the carbide blank
Weigh the tungsten carbide round blank on the 0.01 g scale. Record the mass.
Матеріали для цього кроку:
Graph Paper1 аркушНеобхідні інструменти ({count})
Tungsten Carbide Round Blank 1/2"
Digital Scale (0.01g)Measure its volume by displacement
Measure its volume by displacement
Fill the graduated cylinder to 50 ml, lower the blank in, and read the new level. The difference is its volume in millilitres.
Необхідні інструменти ({count})
Graduated Cylinder (100 ml)
Tungsten Carbide Round Blank 1/2"Calculate the density
Calculate the density
Density = mass ÷ volume. Expect roughly 14-15 g/cm³ for a cobalt-bonded carbide.
Матеріали для цього кроку:
Graph Paper1 аркушНеобхідні інструменти ({count})
Notebook and PencilDo the same for steel
Do the same for steel
Weigh and displace a piece of the mild steel bar. Steel comes out near 7.85 g/cm³.
Матеріали для цього кроку:
Mild Steel Square Bar1 штукаНеобхідні інструменти ({count})
Digital Scale (0.01g)
Graduated Cylinder (100 ml)Compare the two densities
Compare the two densities
Carbide is roughly twice as dense as steel. Tungsten's atomic mass is doing that, and it is your evidence that the blank really is what it claims to be.
Матеріали для цього кроку:
Graph Paper1 аркушНеобхідні інструменти ({count})
Notebook and PencilScratch-test steel with carbide
Scratch-test steel with carbide
Drag a corner of the carbide blank across the mild steel bar with light pressure. It marks the steel easily.
Матеріали для цього кроку:
Mild Steel Square Bar1 штукаНеобхідні інструменти ({count})
Tungsten Carbide Round Blank 1/2"Try the reverse
Try the reverse
Now try to scratch the carbide with an HSS cutter edge. It will not mark. Hardness is one-way, and that asymmetry is the whole ranking.
Необхідні інструменти ({count})
End Mill Set HSS
Tungsten Carbide Round Blank 1/2"
Magnifying GlassBuild a hardness order
Build a hardness order
Test steel, HSS, carbide and glass against each other in pairs and write them in order. You have reconstructed the logic of the Mohs scale from your own bench.
Матеріали для цього кроку:
Graph Paper1 аркушНеобхідні інструменти ({count})
Notebook and PencilLook at a carbide insert's edge
Look at a carbide insert's edge
Inspect an indexable insert under the loupe. Note the blunter included angle compared with HSS — hardness bought with brittleness must be supported by geometry.
Необхідні інструменти ({count})
Indexable Carbide Insert Set (CCMT/TCMT)
Magnifying GlassFind the indexing corners
Find the indexing corners
Count the usable corners on one insert. When one dulls it is rotated, not resharpened — carbide is too hard to grind on an ordinary wheel.
Необхідні інструменти ({count})
Indexable Carbide Insert Set (CCMT/TCMT)
Notebook and PencilTest brittleness safely
Test brittleness safely
Rest the blank on the wooden board and press its edge firmly against the steel bar. Note how unforgiving it feels — carbide chips where steel would deform. Do not strike it.
Матеріали для цього кроку:
Flat Wooden Board1 штука
Mild Steel Square Bar1 штукаНеобхідні інструменти ({count})
Tungsten Carbide Round Blank 1/2"Write the selection rule
Write the selection rule
Interrupted cuts and flexible setups favour HSS; continuous cuts, hard material and high speed favour carbide. Write the rule in your own words.
Матеріали для цього кроку:
Graph Paper1 аркушНеобхідні інструменти ({count})
Notebook and PencilHistory & Context
History & Context
German patent DRP 420,689, Osram Studiengesellschaft, filed 30 March 1923 and published 30 October 1925; method by Karl Schröter. Two things are claimed: a composition — tungsten monocarbide with 10-20 wt% of an iron-group metal — and a manufacturing route, pressing and sintering with a liquid phase present. Krupp acquired the patent in 1926 and launched WIDIA (wie Diamant) in 1927.
Why a lamp company invented a cutting tool. Osram drew tungsten wire for filaments through diamond dies, which were costly and wore out. A synthetic die material was the goal; machining was an application nobody had asked for. The pattern — a material developed for one industry that reshapes another — recurs constantly in materials history.
Cobalt won. The patent lists iron, nickel or cobalt as binder. Cobalt proved best because it wets tungsten carbide grains almost perfectly during liquid-phase sintering, giving a dense body with no voids. Modern grades are still overwhelmingly WC-Co, tuned by grain size and cobalt percentage: more cobalt is tougher and less hard, less cobalt is harder and more brittle.
Why this blueprint does not sinter anything. The process needs powders at 1,400 °C, and fine cobalt powder is a genuine inhalation hazard. Solid sintered carbide — the blank and inserts used here — is inert and safe to handle. The measurements in steps 2-9 establish everything the patent claims about the material without ever making it: density proves the tungsten content, and the scratch order proves the hardness ranking.
What it displaced. High-speed steel (Taylor and White, US 668,270, 1901) gave a tool that survived at 600 °C. Carbide survives past 1,000 °C and cuts several times faster again. It did not replace HSS — drills, taps and end mills for general shop work are still largely HSS, because it can be resharpened and it tolerates flex.
Матеріали
3- 5 аркушівЗаповнювач
- 3 штукЗаповнювач
- 1 штукаЗаповнювач
Необхідні інструменти
7- Заповнювач
- Заповнювач
- Заповнювач
- Заповнювач
- Заповнювач
Матеріали з пов'язаних креслень
Пов'язані креслення
Ці креслення діляться знаннями — техніки, матеріали або принципи
CC0 Суспільне надбання
Це креслення випущено під ліцензією CC0. Ви можете вільно копіювати, змінювати, поширювати та використовувати цю роботу для будь-яких цілей без запиту дозволу.
Підтримайте мейкера, купуючи продукти через його креслення, де він отримує Комісію мейкера встановлену вендорами, або створіть нову ітерацію цього креслення та включіть його як зв'язок у власне креслення для розподілу доходу.