Bonded Wire Strain Gauge on Paper: Simmons, 1942
Edward E. Simmons, Jr. of Pasadena patented the bonded wire strain gauge in 1942, US 2,292,549 (filed 1940). A very fine resistance wire is cemented to a member along its entire length, so it stretches and shortens exactly with the surface and its electrical resistance follows the strain. His preferred form: Constantan or Advance wire, about 0.003 inch, wound back and forth on a thin paper, set in Glyptal, then cemented to the member and calibrated.
Nâng cao
Workshop process
Hướng dẫn
1
1
Wind the filament on thin paper
Wind the filament on thin paper
Use a fine resistance wire such as Constantan or Advance (a copper-nickel alloy, about 45 % nickel and 55 % copper); Simmons used No. 40 gauge, about 0.0031 inch. Wind it back and forth across a thin paper in parallel lengths whose alternate ends are joined, the strands very close together but not touching. A winding jig keeps the filament slightly taut.
Vật liệu cho bước này:
Dây constantan1 as required
Giấy1 tờCông cụ cần thiết:
Đồ gá quấn dây
Kéo2
2
Set it in Glyptal
Set it in Glyptal
Cover the wound filament with Glyptal and let it dry and harden thoroughly. Filament and paper now form one gauge unit, the filament lying in the plane of the paper surface.
Vật liệu cho bước này:
Nhựa alkyd Glyptal1 as requiredCông cụ cần thiết:
Bút vẽ mảnh
Lò sấy3
3
Cement it to the member
Cement it to the member
Put Glyptal on the surface of the member and wrap the gauge unit on with the strands running in the direction of the strain to be measured, the paper outside. The small amount of Glyptal on the surface insulates the filament from the member. Hold filament and paper in place by wrapping them with thread, then dry and harden the Glyptal thoroughly.
Vật liệu cho bước này:
Nhựa alkyd Glyptal1 as required
Chỉ cô tông1 as requiredCông cụ cần thiết:
Bút vẽ mảnh
Lò sấy
Kéo4
4
Calibrate it
Calibrate it
Load the member progressively in a materials testing machine and note the change in the filament's resistance at each load, measured on a Wheatstone bridge in which the filament is one arm. For very fast loads, as in impact tests, an oscillograph takes the place of the galvanometer.
Công cụ cần thiết:
Máy thử vật liệu
Cầu Wheatstone
Điện kế tương tự5
5
Bonding area and signal size
Bonding area and signal size
Đang tải sổ tay Jupyter…
Vật liệu
4- 1 as requiredTạm thời
- 1 tờTạm thời
- 1 as requiredTạm thời
- 1 as requiredTạm thời
Bản thiết kế này làm ra
Blueprint liên quan
Các blueprint này chia sẻ kiến thức — kỹ thuật, vật liệu hoặc nguyên tắc
CC0 Phạm vi công cộng
Bản thiết kế này được phát hành theo CC0. Bạn tự do sao chép, sửa đổi, phân phối và sử dụng cho bất kỳ mục đích nào mà không cần xin phép.
Hỗ trợ nhà sáng tạo bằng cách mua sản phẩm qua bản thiết kế, nơi họ nhận Hoa hồng nhà sáng tạo do nhà bán hàng đặt, hoặc tạo phiên bản mới và kết nối trong bản thiết kế riêng để chia sẻ doanh thu.