Needle File Set: Six Small Files Cut by Hand
Forge

Criado por

Forge

14. outubro 2026NO
27
0
0
0
0

Needle File Set: Six Small Files Cut by Hand

Needle files are small files for fine work, where a good finish matters more than speed, sold in sets of shapes: pillar, half round, barrette, square, round and triangular. They are made like any file, only smaller and with finer teeth: forged, annealed, cut tooth by tooth with a chisel, and hardened in brine. The picture: our diagram, six tapered needle files and their cross-sections.
Avançado
Three days

Instruções

1

Forge six blanks

Draw tool steel to six thin blanks, each with a tapered part for the teeth and a round handle part. Shape the sections in the swage block: pillar (narrow flat), half round, barrette, square, round and triangular.

Materiais para este passo:

Barra octogonal de aço para ferramentasBarra octogonal de aço para ferramentas0.15 kg
Carvão vegetalCarvão vegetal2 as required

Ferramentas necessárias:

Forja de ferreiroForja de ferreiro
BigornaBigorna
Martelo de pena transversalMartelo de pena transversal
Bloco de estamparBloco de estampar
Tenazes de ferreiroTenazes de ferreiro
Luvas de soldadorLuvas de soldador
Óculos de segurançaÓculos de segurança
2

Anneal and true

Anneal the blanks: no hotter than blood red, cooled very slowly out of the air. Grind and file the faces true, or the teeth will not be even.

Ferramentas necessárias:

Forja de ferreiroForja de ferreiro
Mó de afiarMó de afiar
Lima para metalLima para metal
3

Cut the teeth

Raise fine teeth with the file-cutting chisel, one blow and a small even step at a time, under a loupe. Turn each blank on the pewter plate to cut the next face. On the barrette cut only the flat face; leave the other sides smooth (safe).

Ferramentas necessárias:

Talhadeira de picar limasTalhadeira de picar limas
Martelo de pena transversalMartelo de pena transversal
BigornaBigorna
Placa de estanho (peltre)Placa de estanho (peltre)
Lupa de joalheiroLupa de joalheiro
4

Harden, do not temper

Heat each file evenly to its hardening heat and plunge it into cold brine. Then reheat the handle part alone so it is not glass-hard.

Materiais para este passo:

SalSal0.5 kg
ÁguaÁgua5 litros

Ferramentas necessárias:

Forja de ferreiroForja de ferreiro
BaldeBalde
Tenazes de ferreiroTenazes de ferreiro
Luvas de soldadorLuvas de soldador
Óculos de segurançaÓculos de segurança
5

Steel for a set of six

A carregar o notebook Jupyter…

Materiais

4

Ferramentas necessárias

13

Blueprints relacionados

Estes blueprints compartilham conhecimento — técnicas, materiais ou princípios

CC0 Domínio Público

Este blueprint é liberado sob CC0. Você é livre para copiar, modificar, distribuir e usar este trabalho para qualquer finalidade, sem pedir permissão.

Apoie o Maker comprando produtos através do Blueprint, onde ele ganha uma Comissão Maker definida pelos vendedores, ou crie uma nova versão deste Blueprint e inclua-o como conexão no seu próprio Blueprint para compartilhar receita.

Discussão

(0)

Entrar para participar da discussão

Carregando comentários...