Anti-Reflection Coating

Katharine Blodgett at General Electric, working with Irving Langmuir, learned to build soap-like films one molecule-thick layer at a time. Stacking just enough layers onto glass, she made it nearly invisible: light reflected from the top of the film and from the glass beneath cancelled out. **US 2,220,861**, "Reduction of surface reflection", Blodgett, assigned to General Electric, filed 16. June 1938, granted 5. November 1940: a coating whose "optical thickness … corresponds at least approximately to a quarter wave length of visible light" and whose refractive index is "intermediate" between air and the glass. **You measure the reflection a coating removes**, design one in a notebook, and watch quarter-wave interference happen in a soap film.
Débutant
90 minutes

Consignes

1

Measure bare glass

Clip the solar cell to the multimeter (DC mA). In a dim room shine the laser straight onto the cell and note the current. Then bounce the beam off a clean microscope slide, close to perpendicular, onto the cell. Note that current. Never look along the beam.

Matériaux pour cette étape :

Lames de microscope avec lamellesLames de microscope avec lamelles1 paquet
Solar Cell Mini - 350mVSolar Cell Mini - 350mV1 pièce

Outils nécessaires :

Pointeur laserPointeur laser
MultimètreMultimètre
Alligator to Alligator CablesAlligator to Alligator Cables
2

Mix a film solution

Stir 1 part detergent and 1 part glycerin into 10 parts water in a jar. Bend copper wire into a 60 mm loop with a handle.

Matériaux pour cette étape :

Détergent douxDétergent doux20 ml
Glycérine (végétale)Glycérine (végétale)20 ml
Fil de cuivreFil de cuivre1 mètre

Outils nécessaires :

Bocal en verreBocal en verre
Jeu de pincesJeu de pinces
3

Watch a film thin

Dip the loop and hold it upright in front of black card, lit by a window behind you. Colour bands slide down as the film drains; at the top a black band appears - a film too thin to reflect.

Matériaux pour cette étape :

Carton noirCarton noir1 feuille
4

Fresnel, coating design, soap film

Chargement du notebook Jupyter…
5

History & Context

**What the patent specifies:** a surface layer of quarter-wave optical thickness with a refractive index between those of the surrounding medium and the glass. **Modern build (derived):** measurement and design only - production coatings are evaporated in vacuum. Blodgett's stearate films were too soft to wipe clean. Alexander Smakula at Zeiss had developed coatings evaporated in vacuum in 1935; that durable route won, and today almost every camera lens and eyeglass is coated, often with many layers. Their limits: a single layer is perfect at only one wavelength, and coatings scratch.
Étape 5 - Image 1

Matériaux

6

Outils requis

5
Total estimé
Ce que le maker a acheté. Les matériaux sans prix se trouvent là où vous les achetez.
€1.93

Blueprints liés

Ces blueprints partagent des connaissances — techniques, matériaux ou principes

CC0 Domaine public

Ce blueprint est publié sous CC0. Vous êtes libre de copier, modifier, distribuer et utiliser ce travail pour tout usage, sans demander la permission.

Soutenez le Maker en achetant des produits via son Blueprint où il perçoit une Commission Maker définie par les Vendeurs, ou créez une nouvelle itération de ce Blueprint et incluez-le comme connexion dans votre propre Blueprint pour partager les revenus.

Commentaires

(0)

Se connecter pour participer à la discussion

Chargement des commentaires...