Running a Bead: Travel Speed Is Not a Matter of Taste
Forge

Créé par

Forge

24. septembre 2026NO
23
0
0
0
0

Running a Bead: Travel Speed Is Not a Matter of Taste

A bead is a line of weld metal laid down in one pass. It is the unit everything else is built out of, and it is where a welder is taught, because a bead run on a flat plate with no joint under it shows every fault without hiding any of them. Three things are read off a finished bead: its width, its height, and the row of ripples on top. Each of those reports on one of the variables from the previous rung. This rung also works out heat input in joules per millimetre — the number that connects current, arc voltage and travel speed, and the one that decides how far the work will pull out of shape.
Débutant
4 hours

Consignes

1

What a bead is telling you

**Width** reports arc length and weave. A bead two to three times the core diameter is a stringer, run straight. Much wider than that on a straight run means the arc is too long. **Height** reports travel speed. Too slow and the metal piles up into a tall, narrow, rope-like bead that has barely fused into the plate beneath it. Too fast and the bead is thin, stringy and often has a crack down the middle of the crater at the end. **The ripples** report steadiness. Even crescents, evenly spaced, all pointing backwards, mean a steady speed and a steady arc. Ripples that bunch and stretch mean a hand that is speeding up and slowing down. A bead that is about twice as wide as it is high, flat-faced or slightly convex, blending into the plate at both toes without a sharp step, is a good one.

Matériaux pour cette étape :

Plaque d'acier douxPlaque d'acier doux2 pièces
Électrode de soudageÉlectrode de soudage1 paquet

Outils nécessaires :

Poste à souder à l'arcPoste à souder à l'arc
Masque de soudage à obscurcissement automatiqueMasque de soudage à obscurcissement automatique
Gants de soudeurGants de soudeur
Loupe de bijoutierLoupe de bijoutier
2

Heat input, and why the speed is already decided

Chargement du notebook Jupyter…

Outils nécessaires :

Ordinateur de bureauOrdinateur de bureau
3

Stringer or weave

A **stringer** is run straight along the joint with no side-to-side movement. It puts less heat into the plate per unit length of joint, cools faster, and is what you want on thin material, on high-strength steels, and for the root run of a multi-pass weld. A **weave** swings the rod side to side to fill a wider gap in one pass. It is slower along the joint, so it puts in much more heat, and it is the right answer for filling a wide V and for capping a multi-pass weld. The practical limit on a weave is about two and a half to three times the core diameter of the electrode. Wider than that and the pool is too big for the arc to hold — it sags in the flat position and simply falls out in any other. Pause very slightly at each edge of a weave. That is where the pool has to wash into the parent metal, and a weave that sweeps straight through leaves cold, unfused edges under a bead that looks fine from the top.

Matériaux pour cette étape :

Plaque d'acier douxPlaque d'acier doux2 pièces
Électrode de soudageÉlectrode de soudage1 paquet

Outils nécessaires :

Poste à souder à l'arcPoste à souder à l'arc
Masque de soudage à obscurcissement automatiqueMasque de soudage à obscurcissement automatique
Gants de soudeurGants de soudeur
4

Starting, restarting and filling the crater

The two weakest points of a bead are its two ends. **At the start** the plate is cold, so the first 10-20 mm gets less penetration than the rest. Strike about 10 mm ahead of where the weld is to begin, run back to the start, then go forward over the strike point — by the time you cross it the plate is warm. **At a restart** the old crater must be chipped and brushed clean of slag first. Restart on the front edge of the crater, hold long enough to fill it, then move on. Restarting on top of slag is the commonest way to bury an inclusion. **At the end** stopping dead leaves a crater — a dish of metal that has solidified last, fed by nothing, and it very often cracks down the middle. Fill it: pause, or swing back over the last 10 mm of the bead before lifting away.

Matériaux pour cette étape :

Plaque d'acier douxPlaque d'acier doux2 pièces
Électrode de soudageÉlectrode de soudage1 paquet

Outils nécessaires :

Poste à souder à l'arcPoste à souder à l'arc
Masque de soudage à obscurcissement automatiqueMasque de soudage à obscurcissement automatique
Gants de soudeurGants de soudeur
MarteauMarteau
Jeu de brosses métalliquesJeu de brosses métalliques
Barre à tisonner la scorieBarre à tisonner la scorie

Matériaux

2

Outils requis

8

CC0 Domaine public

Ce blueprint est publié sous CC0. Vous êtes libre de copier, modifier, distribuer et utiliser ce travail pour tout usage, sans demander la permission.

Soutenez le Maker en achetant des produits via son Blueprint où il perçoit une Commission Maker définie par les Vendeurs, ou créez une nouvelle itération de ce Blueprint et incluez-le comme connexion dans votre propre Blueprint pour partager les revenus.

Commentaires

(0)

Se connecter pour participer à la discussion

Chargement des commentaires...