Forged Geologist's Pick
A geologist's pick of about 2½ pounds, with a square striking head on one side of the eye and a long curved point on the other, forged from 1¼ × 1¾-inch tool steel. After the eye is punched, the bar is cut part way through beside it with a hot chisel and the waste cut away, then each end is drawn out, under a power hammer in the original. The point is hardened like a cold chisel and tempered to dark blue; the head is then hardened about 2 inches back and tempered to brown or dark straw, with damp coal round the point so it is not softened again.
Lanjutan
4–6 hours
Arahan
1
1
Mark and punch
Mark and punch
Mark the stock with a centre punch and chisel, and punch the hole for the eye.
Bahan untuk langkah ini:
Bar keluli alat leper1 kepingAlatan diperlukan:
Penebuk Pusat
Relau tukang besi
Andas
Penebuk panas
Penyepit tukang besi2
2
Cut beside the eye
Cut beside the eye
With a drift in the eye, flatten the sides. Cut part way through 3/16 inch from the edge of the hole on both sides, round the bottom of the cuts with a thin fuller, and cut out the waste.
Alatan diperlukan:
Pelebar lubang tirus
Pahat panas
Fuller (besi pembuat lurah)3
3
Draw out the ends
Draw out the ends
Draw out one end, cut the pick from the bar, then draw out the other end to the point's form.
Alatan diperlukan:
Tukul jatuh
Tukul besar4
4
Finish the head and point
Finish the head and point
With the drift in the eye, smooth around it with a set hammer. Finish the head with set hammer and flatter and cut it square from four sides; finish the point with a flatter and cut it to length. Grind face and point.
Alatan diperlukan:
Tukul set tukang besi
Perata tempaan
Pahat panas
Pengisar meja5
5
Harden and temper
Harden and temper
Harden the point like a cold chisel and temper it to dark blue. Then heat about 2 inches of the head, keeping damp coal around the point, harden it the same way and temper it to brown or dark straw.
Alatan diperlukan:
Relau tukang besi
Baldi pelindapkejutan
Penyepit tukang besi
Kain emeri6
6
Handle
Handle
Shave the handle stock to fit the eye tightly, drive the head on, saw a kerf in the handle's top and drive a glued hardwood wedge into it. Trim flush and oil the handle.
Bahan untuk langkah ini:
Batang Kayu Keras untuk Hulu1 keping
Pasak kayu keras1 keping
Minyak Biji Rami10 mlAlatan diperlukan:
Ketam lengkung
Gergaji rentas dua orang
Ragum BangkuBahan
4- 1 kepingPemegang Tempat
- 1 kepingPemegang Tempat
- 1 kepingPemegang Tempat
- 10 mlPemegang Tempat
Alatan Diperlukan
18- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
- Pemegang Tempat
Blueprint ini membuat
Blueprint berkaitan
Blueprint ini berkongsi pengetahuan — teknik, bahan atau prinsip
CC0 Domain Awam
Blueprint ini dikeluarkan di bawah CC0. Anda bebas menyalin, mengubah, mengedar, dan menggunakan karya ini untuk sebarang tujuan, tanpa meminta kebenaran.
Sokong Pembuat dengan membeli produk melalui Blueprint mereka di mana mereka memperoleh Komisen Pembuat ditetapkan oleh Penjual, atau cipta iterasi baru Blueprint ini dan sertakan ia sebagai sambungan dalam Blueprint anda sendiri untuk berkongsi hasil.