Precipitated Silver: Silver Chloride Reduced by Zinc in Acidulated Water (Thorpe 1913)

Precipitated Silver: Silver Chloride Reduced by Zinc in Acidulated Water (Thorpe 1913)

autor: CharlieDE

Organiczny

1
0
0
0
0
0
Dextrin: Starch Moistened with Dilute Nitric Acid and Heated at 110-120 °C (Payen, in Thorpe 1912)

Dextrin: Starch Moistened with Dilute Nitric Acid and Heated at 110-120 °C (Payen, in Thorpe 1912)

autor: CharlieDE

Organiczny

0
0
0
0
0
0
Silver Oxide: Silver Nitrate Precipitated with Solution of Potassa (USP 1870)

Silver Oxide: Silver Nitrate Precipitated with Solution of Potassa (USP 1870)

autor: CharlieDE

Organiczny

4
0
0
0
0
0
Ferrite Toroid Core: Nickel-Zinc Ferrite Given a Further Oxygen Treatment (Snoek 1948, Ex. IV)
Niebezpieczne

Ferrite Toroid Core: Nickel-Zinc Ferrite Given a Further Oxygen Treatment (Snoek 1948, Ex. IV)

autor: CharlieDE

Organiczny

3
0
0
0
0
0
Ferrite Toroid Core: Magnesium-Zinc Ferrite Reheated 18 h at 1000 °C and 20 h at 750 °C (Snoek 1948, Ex. III)

Ferrite Toroid Core: Magnesium-Zinc Ferrite Reheated 18 h at 1000 °C and 20 h at 750 °C (Snoek 1948, Ex. III)

autor: CharlieDE

Organiczny

2
0
0
0
0
0
Ferrite Toroid Core: Wet-Process Copper-Zinc Ferrite with a Stepped Anneal Down to 310 °C (Snoek 1948)

Ferrite Toroid Core: Wet-Process Copper-Zinc Ferrite with a Stepped Anneal Down to 310 °C (Snoek 1948)

autor: CharlieDE

Organiczny

2
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite by the Wet Process, Precipitated with Caustic Soda (Snoek 1948)

Ferrite Toroid Core: Copper-Zinc Ferrite by the Wet Process, Precipitated with Caustic Soda (Snoek 1948)

autor: CharlieDE

Organiczny

3
0
0
0
0
0
Ferrite Toroid Core: Copper-Cadmium Ferrite, 200-Hour Grind, 1000 °C in Oxygen (Snoek 1948, Ex. I)
Niebezpieczne

Ferrite Toroid Core: Copper-Cadmium Ferrite, 200-Hour Grind, 1000 °C in Oxygen (Snoek 1948, Ex. I)

autor: CharlieDE

Organiczny

1
0
0
0
0
0
Cadmium Oxide: Cadmium Heated in a Current of Oxygen (Thorpe 1912)
Niebezpieczne

Cadmium Oxide: Cadmium Heated in a Current of Oxygen (Thorpe 1912)

autor: CharlieDE

Organiczny

3
0
0
0
0
0
Ferric Nitrate: Scrap Iron Dissolved in Concentrated Nitric Acid (Thorpe 1912)
Niebezpieczne

Ferric Nitrate: Scrap Iron Dissolved in Concentrated Nitric Acid (Thorpe 1912)

autor: CharlieDE

Organiczny

3
0
0
0
0
0
Antimony Trioxide: Roasted Antimony Fused with More Metal (Thorpe 1912)

Antimony Trioxide: Roasted Antimony Fused with More Metal (Thorpe 1912)

autor: CharlieDE

Organiczny

3
0
0
0
0
0
Extruded Polystyrene Foam: Butylene-Blown Logs 20 Inches Across (McIntire, Dow 1948, Ex. 4)

Extruded Polystyrene Foam: Butylene-Blown Logs 20 Inches Across (McIntire, Dow 1948, Ex. 4)

autor: CharlieDE

Organiczny

1
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 75 °C (McIntire, Dow 1948, Ex. 3, Test 4)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 75 °C (McIntire, Dow 1948, Ex. 3, Test 4)

autor: CharlieDE

Organiczny

1
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 60 °C (McIntire, Dow 1948, Ex. 3, Test 3)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 60 °C (McIntire, Dow 1948, Ex. 3, Test 3)

autor: CharlieDE

Organiczny

2
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 50 °C (McIntire, Dow 1948, Ex. 3, Test 2)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 50 °C (McIntire, Dow 1948, Ex. 3, Test 2)

autor: CharlieDE

Organiczny

1
0
0
0
0
0
Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 40 °C (McIntire, Dow 1948, Ex. 3, Test 1)

Extruded Polystyrene Foam: Propylene-Blown Log Let Out at 40 °C (McIntire, Dow 1948, Ex. 3, Test 1)

autor: CharlieDE

Industry 3.0 — Assembly Line & Mass Production (1913)

1
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 100 °C (McIntire, Dow 1948, Ex. 2)
Niebezpieczne

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 100 °C (McIntire, Dow 1948, Ex. 2)

autor: CharlieDE

Organiczny

1
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 90 °C (McIntire, Dow 1948, Ex. 2)
Niebezpieczne

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 90 °C (McIntire, Dow 1948, Ex. 2)

autor: CharlieDE

Organiczny

2
0
0
0
0
0
Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 80 °C (McIntire, Dow 1948, Ex. 2)
Niebezpieczne

Extruded Polystyrene Foam: Methyl and Methylene Chloride Gel Let Out at 80 °C (McIntire, Dow 1948, Ex. 2)

autor: CharlieDE

Organiczny

2
0
0
0
0
0
Dichloromethane: Chloroform Reduced with Zinc, Alcohol and Hydrochloric Acid (Greene, in Thorpe 1912)
Niebezpieczne

Dichloromethane: Chloroform Reduced with Zinc, Alcohol and Hydrochloric Acid (Greene, in Thorpe 1912)

autor: CharlieDE

Organiczny

2
0
0
0
0
0
Lead Dioxide: Red Lead Treated with Nitric Acid (Thorpe 1912)
Niebezpieczne

Lead Dioxide: Red Lead Treated with Nitric Acid (Thorpe 1912)

autor: CharlieDE

Organiczny

1
0
0
0
0
0
Cadmium Sulphide: Precipitated from a Cadmium Salt with an Alkaline Sulphide (Thorpe 1912)
Niebezpieczne

Cadmium Sulphide: Precipitated from a Cadmium Salt with an Alkaline Sulphide (Thorpe 1912)

autor: CharlieDE

Organiczny

3
0
0
0
0
0
Cadmium Chloride: Cadmium Dissolved in Hydrochloric Acid and Evaporated (Thorpe 1912)
Niebezpieczne

Cadmium Chloride: Cadmium Dissolved in Hydrochloric Acid and Evaporated (Thorpe 1912)

autor: CharlieDE

Organiczny

1
0
0
0
0
0
Strontium Carbonate: Powdered Celestine Boiled with Soda Solution (Thorpe 1912)

Strontium Carbonate: Powdered Celestine Boiled with Soda Solution (Thorpe 1912)

autor: CharlieDE

Organiczny

2
0
0
0
0
0
Pokazano 24 z 128