Nitric Acid: Chile Saltpetre Distilled with Oil of Vitriol in an Iron Retort
危険

Nitric Acid: Chile Saltpetre Distilled with Oil of Vitriol in an Iron Retort

Charlie 作DE

化学

1
0
0
0
0
0
Oxalic Acid: Wood Soaked in Caustic Alkali and Heated in Hot Air at 300 °C (Plater-Syberg)
危険

Oxalic Acid: Wood Soaked in Caustic Alkali and Heated in Hot Air at 300 °C (Plater-Syberg)

Charlie 作DE

化学

6
0
0
0
0
0
Oxalic Acid: Sawdust Heated with Alkali Lye in Vacuum, Oxidised, Precipitated as Calcium Oxalate (Zacher)
危険

Oxalic Acid: Sawdust Heated with Alkali Lye in Vacuum, Oxidised, Precipitated as Calcium Oxalate (Zacher)

Charlie 作DE

化学

2
0
0
0
0
0
Diethyl Ether: Soubeiran's One-Operation Still with a Caustic Charcoal Purifier
危険

Diethyl Ether: Soubeiran's One-Operation Still with a Caustic Charcoal Purifier

Charlie 作DE

化学

2
0
0
0
0
0
Urea: Extracted from Urine with Alcohol, Precipitated as the Nitrate, Freed with Barium Carbonate
危険

Urea: Extracted from Urine with Alcohol, Precipitated as the Nitrate, Freed with Barium Carbonate

Charlie 作DE

化学

1
0
0
0
0
0
Urea: Separated from Urine as the Oxalate, Freed with Chalk and Crystallised

Urea: Separated from Urine as the Oxalate, Freed with Chalk and Crystallised

Charlie 作DE

化学

4
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Milled 200 Hours, Fired at 1050 °C (Snoek)

Ferrite Toroid Core: Copper-Zinc Ferrite Milled 200 Hours, Fired at 1050 °C (Snoek)

Charlie 作DE

化学

2
0
0
0
0
0
Ferrite Toroid Core: Magnesium-Zinc Ferrite (28 : 18 : 54) Fired at 1400 °C (Snoek)

Ferrite Toroid Core: Magnesium-Zinc Ferrite (28 : 18 : 54) Fired at 1400 °C (Snoek)

Charlie 作DE

化学

4
0
0
0
0
0
Ferrite Toroid Core: Nickel-Zinc Ferrite Fired at 1400 °C, Held at 930 °C (Snoek)
危険

Ferrite Toroid Core: Nickel-Zinc Ferrite Fired at 1400 °C, Held at 930 °C (Snoek)

Charlie 作DE

化学

5
0
0
0
0
0
Ferrite Toroid Core: Copper-Zinc Ferrite Fired at 1050 °C, Held at 600 °C in Oxygen (Snoek)

Ferrite Toroid Core: Copper-Zinc Ferrite Fired at 1050 °C, Held at 600 °C in Oxygen (Snoek)

Charlie 作DE

化学

4
0
0
0
0
0
Ferrite Toroid Core: Magnesium-Zinc Ferrite Fired at 1300 °C in Oxygen (Snoek)

Ferrite Toroid Core: Magnesium-Zinc Ferrite Fired at 1300 °C in Oxygen (Snoek)

Charlie 作DE

化学

4
0
0
0
0
0
Ferrite Toroid Core: Magnesium-Zinc Ferrite Fired at 1400 °C in Oxygen (Snoek)

Ferrite Toroid Core: Magnesium-Zinc Ferrite Fired at 1400 °C in Oxygen (Snoek)

Charlie 作DE

化学

2
0
0
0
0
0
Laminated Phenolic Paper Sheet: Bakelite-Coated Kraft Paper Hot-Pressed and Baked (O'Conor, Westinghouse 1918)
危険

Laminated Phenolic Paper Sheet: Bakelite-Coated Kraft Paper Hot-Pressed and Baked (O'Conor, Westinghouse 1918)

Charlie 作DE

化学

3
0
0
0
0
0
Liquid Bakelite: Phenol and Formalin Heated Together, the Oily Layer Kept (Baekeland 1909)
危険

Liquid Bakelite: Phenol and Formalin Heated Together, the Oily Layer Kept (Baekeland 1909)

Charlie 作DE

化学

3
0
0
0
0
0
Ferrite Toroid Core: Nickel-Zinc Ferrite Sintered at 1300 °C in Oxygen (Snoek)
危険

Ferrite Toroid Core: Nickel-Zinc Ferrite Sintered at 1300 °C in Oxygen (Snoek)

Charlie 作DE

化学

5
0
0
0
0
0
Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Acetic acid

Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Acetic acid

Charlie 作DE

化学

3
0
0
0
0
0
Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Acetone

Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Acetone

Charlie 作DE

化学

3
0
0
0
0
0
Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Isopropanol

Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Isopropanol

Charlie 作DE

化学

2
0
0
0
0
0
Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Methanol

Acrylic Mirror Sheet: Silver Sprayed on Acrylic Treated with Tannin in Water and Methanol

Charlie 作DE

化学

4
0
0
0
0
0
Diethyl Ether: Alcohol Dropped into Sulphuric Acid at 130–140 °C (Boullay's Continuous Method)
危険

Diethyl Ether: Alcohol Dropped into Sulphuric Acid at 130–140 °C (Boullay's Continuous Method)

Charlie 作DE

化学

5
0
0
0
0
0
Tannic Acid: Galls Stirred to a Cream with Ether and Pressed (Leconnet)

Tannic Acid: Galls Stirred to a Cream with Ether and Pressed (Leconnet)

Charlie 作DE

化学

2
0
0
0
0
0
Tannic Acid: Powdered Galls Extracted with Ether and Alcohol (75:25)

Tannic Acid: Powdered Galls Extracted with Ether and Alcohol (75:25)

Charlie 作DE

化学

2
0
0
0
0
0
Tannic Acid: Chinese Galls Extracted with Warm Water, Shaken with Ether and Dried on Tin Sheets

Tannic Acid: Chinese Galls Extracted with Warm Water, Shaken with Ether and Dried on Tin Sheets

Charlie 作DE

化学

3
0
0
0
0
0
Acrylic Mirror Sheet: Silver Sprayed on Tannin-Treated Acrylic

Acrylic Mirror Sheet: Silver Sprayed on Tannin-Treated Acrylic