Barium-Calcium Ferrite Disc Magnet: Equal Barium and Calcium, Sintered at 1280 °C (Went, Philips 1956, Ex. 22)

Barium-Calcium Ferrite Disc Magnet: Equal Barium and Calcium, Sintered at 1280 °C (Went, Philips 1956, Ex. 22)

por CharlieDE

Materiais

0
0
0
0
0
0
Barium-Calcium Ferrite Disc Magnet: Part of the Barium Replaced by Calcium (Went, Philips 1956, Ex. 21)

Barium-Calcium Ferrite Disc Magnet: Part of the Barium Replaced by Calcium (Went, Philips 1956, Ex. 21)

por CharlieDE

Materiais

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Chromic Oxides, 1350 °C (Masuyama 1972, Ex. 3)

Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Chromic Oxides, 1350 °C (Masuyama 1972, Ex. 3)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Titanium Oxides, 1350 °C (Masuyama 1972, Ex. 3)

Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Titanium Oxides, 1350 °C (Masuyama 1972, Ex. 3)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Barium Oxides, 1350 °C (Masuyama 1972, Ex. 3)

Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Barium Oxides, 1350 °C (Masuyama 1972, Ex. 3)

por EdFI

Industrial

0
0
0
0
0
0
Barium Ferrite Disc Magnet, Sintered at 1300 °C (Went, Philips 1956)

Barium Ferrite Disc Magnet, Sintered at 1300 °C (Went, Philips 1956)

por CharlieDE

Materiais

0
0
0
0
0
0
Barium Ferrite Disc Magnet, Sintered at 1200 °C (Went, Philips 1956)

Barium Ferrite Disc Magnet, Sintered at 1200 °C (Went, Philips 1956)

por CharlieDE

Materiais

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth and Aluminium Oxides, 1350 °C (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with Bismuth and Aluminium Oxides, 1350 °C (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth and Titanium Oxides, 1350 °C (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with Bismuth and Titanium Oxides, 1350 °C (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth and Nickel Oxides, 1350 °C (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with Bismuth and Nickel Oxides, 1350 °C (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth and Tin Oxides, 1350 °C (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with Bismuth and Tin Oxides, 1350 °C (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth and Barium Oxides, 1350 °C (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with Bismuth and Barium Oxides, 1350 °C (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth and Chromic Oxides, 1350 °C (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with Bismuth and Chromic Oxides, 1350 °C (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with Bismuth and Manganese Oxides, 1350 °C (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with Bismuth and Manganese Oxides, 1350 °C (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with 0.1 % Bismuth Oxide, 1100 °C, 1.0 mm (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with 0.1 % Bismuth Oxide, 1100 °C, 1.0 mm (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 1000 °C, 0.5 mm (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 1000 °C, 0.5 mm (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Metal Oxide Varistor: Zinc Oxide with 0.5 % Bismuth Oxide, 1100 °C, 1.0 mm (Masuyama 1972)

Metal Oxide Varistor: Zinc Oxide with 0.5 % Bismuth Oxide, 1100 °C, 1.0 mm (Masuyama 1972)

por EdFI

Industrial

0
0
0
0
0
0
Neodymium Magnets, Sample 21: 75Fe-8B-17Nd Sintered (Sagawa 1988)

Neodymium Magnets, Sample 21: 75Fe-8B-17Nd Sintered (Sagawa 1988)

por ForgeNO

Trabalho em Metal

2
0
0
0
0
0
Neodymium Magnets, Sample 19: 79Fe-8B-13Nd Sintered (Sagawa 1988)

Neodymium Magnets, Sample 19: 79Fe-8B-13Nd Sintered (Sagawa 1988)

por ForgeNO

Trabalho em Metal

2
0
0
0
0
0
Neodymium Magnets, Sample 8: 75Fe-10B-15Nd Sintered (Sagawa 1988)

Neodymium Magnets, Sample 8: 75Fe-10B-15Nd Sintered (Sagawa 1988)

por ForgeNO

Trabalho em Metal

2
0
0
0
0
0
Neodymium Magnets, Sample 7: 77Fe-8B-15Nd Sintered (Sagawa 1988)

Neodymium Magnets, Sample 7: 77Fe-8B-15Nd Sintered (Sagawa 1988)

por ForgeNO

Trabalho em Metal

2
0
0
0
0
0
Neodymium Magnets, Sample 4: 81Fe-4B-15Nd Sintered (Sagawa 1988)

Neodymium Magnets, Sample 4: 81Fe-4B-15Nd Sintered (Sagawa 1988)

por ForgeNO

Trabalho em Metal

1
0
0
0
0
0
Neodymium Magnets, Sample 20: 78Fe-8B-14Nd Sintered (Sagawa 1988)

Neodymium Magnets, Sample 20: 78Fe-8B-14Nd Sintered (Sagawa 1988)

por ForgeNO

Trabalho em Metal

2
0
0
0
0
0
Neodymium Magnets, Sample 6: 78Fe-7B-15Nd Sintered (Sagawa 1988)