Industry 4.0 — Computers & Digital Automation (1960)
203 blueprint ang available
Mga Blueprint (203)

Barium-Calcium Ferrite Disc Magnet: 20 % Calcium, 5 Minutes at 1290 °C (Went, Philips 1956, Ex. 20)
ni Charlie
Mga Materyales
4
0
0
0
0
0

Barium-Calcium Ferrite Disc Magnet: 5 % Calcium, Sintered at 1330 °C (Went, Philips 1956, Ex. 18)
ni Charlie
Mga Materyales
2
0
0
0
0
0

Barium Ferrite Disc Magnet: Fired in Carbon Dioxide, Pressed at 12 t/cm² (Went, Philips 1956, Ex. 33)
ni Charlie
Mga Materyales
6
0
0
0
0
0

Barium-Calcium Ferrite Disc Magnet: Equal Barium and Calcium, Sintered at 1280 °C (Went, Philips 1956, Ex. 22)
ni Charlie
Mga Materyales
5
0
0
0
0
0

Barium-Calcium Ferrite Disc Magnet: Part of the Barium Replaced by Calcium (Went, Philips 1956, Ex. 21)
ni Charlie
Mga Materyales
4
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Chromic Oxides, 1350 °C (Masuyama 1972, Ex. 3)
ni Ed
Industriyal
2
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Titanium Oxides, 1350 °C (Masuyama 1972, Ex. 3)
ni Ed
Industriyal
4
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth, Manganese and Barium Oxides, 1350 °C (Masuyama 1972, Ex. 3)
ni Ed
Industriyal
3
0
0
0
0
0

Barium Ferrite Disc Magnet, Sintered at 1300 °C (Went, Philips 1956)
ni Charlie
Mga Materyales
5
0
0
0
0
0

Barium Ferrite Disc Magnet, Sintered at 1200 °C (Went, Philips 1956)
ni Charlie
Mga Materyales
3
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth and Aluminium Oxides, 1350 °C (Masuyama 1972)
ni Ed
Industriyal
2
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth and Titanium Oxides, 1350 °C (Masuyama 1972)
ni Ed
Industriyal
2
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth and Nickel Oxides, 1350 °C (Masuyama 1972)
ni Ed
Industriyal
1
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth and Tin Oxides, 1350 °C (Masuyama 1972)
ni Ed
Industriyal
2
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth and Barium Oxides, 1350 °C (Masuyama 1972)
ni Ed
Industriyal
1
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth and Chromic Oxides, 1350 °C (Masuyama 1972)
ni Ed
Industriyal
3
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with Bismuth and Manganese Oxides, 1350 °C (Masuyama 1972)
ni Ed
Industriyal
1
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with 0.1 % Bismuth Oxide, 1100 °C, 1.0 mm (Masuyama 1972)
ni Ed
Industriyal
2
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with 0.2 % Bismuth Oxide, 1000 °C, 0.5 mm (Masuyama 1972)
ni Ed
Industriyal
0
0
0
0
0
0

Metal Oxide Varistor: Zinc Oxide with 0.5 % Bismuth Oxide, 1100 °C, 1.0 mm (Masuyama 1972)
ni Ed
Industriyal
1
0
0
0
0
0

Neodymium Magnets, Sample 21: 75Fe-8B-17Nd Sintered (Sagawa 1988)
ni Forge
Paggawa ng Metal
3
0
0
0
0
0

Neodymium Magnets, Sample 19: 79Fe-8B-13Nd Sintered (Sagawa 1988)
ni Forge
Paggawa ng Metal
1
0
0
0
0
0

Neodymium Magnets, Sample 8: 75Fe-10B-15Nd Sintered (Sagawa 1988)
ni Forge
Paggawa ng Metal
7
0
0
0
0
0

Neodymium Magnets, Sample 7: 77Fe-8B-15Nd Sintered (Sagawa 1988)
ni Forge
Paggawa ng Metal
6
0
0
0
0
0
Ipinapakita ang 24 sa 203